Property |
Units |
State |
||
UnfiredGood thermal shock properties |
Ceramit 10Fired 800-1000°C Good thermal shock properties |
Ceramit 14Fired 1300°C Excellent electrical properties |
||
|
Density |
g/cm3 |
- |
- |
2.4-2.55 |
|
Colour |
Grey |
Pink to Dark Brown |
||
|
Hardness |
Mohs |
2.5 |
5 |
7 |
|
Porosity |
% |
1.8-2 |
2.66 ± 0.02 |
0.01-Nil |
|
|
||||
|
Softening Temperature |
°C |
- |
1600°C |
|
|
Max.Continuous Temp. |
°C |
- |
1100°C |
|
|
Coefficient of linear thermal Expansion |
X 10-6 20 - 600°C |
- |
2.9-3.5 |
6-8 |
|
Thermal Conductivity |
W/mK |
1.5 |
1.9 |
|
|
Compressive strength |
KN/cm² |
- |
10.3 |
15.16 |
|
Cross bending strength |
1.13 -1.58 |
3.37 |
8.27 |
|
|
Tensile strength |
1.03 |
2.34 |
3.44 |
|
|
Volume resistivity |
20 300 500 MΩ/cm3 700 900 |
- - - - - |
Same As Ceramit14 When dry |
1014 109 106 105 104 |
|
Dielectric Strength |
Kv (Using a 5mm thick test piece) |
- |
- |
24 |
|
Power Factor |
@1mHz tand x 104 |
- |
- |
0.1 - 0.13 |
|
Permitivity |
- |
- |
5.2 |
|
|
T E Value |
°C |
- |
- |
700 |
|
Loss Factor |
1000K/Hz |
- |
- |
0.05 |
Copyright ©
Ceramic Substrates & Components Ltd - all copyrights
and other intellectual property rights of this web site are reserved. Any copying
of the design or contents or other unauthorised use will infringe the rights
of Ceramic Substrates & Components Ltd under international treaty and English
law.
Website usage terms and conditions | Sitemap